NOMINAL DATA SHEET


TYPICAL CHEMISTRY
MOLYBDENUM
99.9% (minimum)
POTASSIUM
.0007
ALUMINUM
.0005
SILICON
.0050
IRON
.0040
NICKEL
.0030
COPPER
.0001
CHROMIUM
.0001
SODIUM
.0001
TUNGSTEN
.0020

 

TYPICAL PROPERTIES
ATOMIC WEIGHT
95.94
THERMAL CONDUCTIVITY
DENSTIY
10.14 gm/cm3
20 C
0.34 cal/cm/s/ C
MELTING POINT 2610 +/-10 C
1000 C
0.25 cal/cm/s/ C
RECRYSTALLIZATION
1500 C
0.22 cal/cm/s/ C
TEMPERATURE (100%)
2200 C
0.17 cal/cm/s/ C
RECRYSTALLIZATION
1000 to 1100 C
SPECIFIC HEAT
TRANSITION POINT
20 C
6.2 x 10-2 cal/gm/ C
BRITTLE/DUCTILE
-100 to 100 C
1000 C
7.4 x 10-2 cal/gm/ C
VAPOR PRESSURE
2000 C
10.0 x 10-2 cal/gm/ C
1500 C
6.4 x 10-9 mm Hg
RESTIVITY
2000 C
4.0 x 10-5 mm Hg
20 C
5.3 x 10-6 ohm-cm
2500 C
1.0 x 10-2 mm Hg
1000 C
3.2 x 10-5 ohm-cm
COEFFICIENT OF LINEAR EXPANSION
2000 C
6.1 x 10-5 ohm-cm
20 C
5.3 x 10-6 C-1
TEMPERATURE
20-1000 C
5.8 x 10-6 C-1
COEFFICIENT
20-1500 C
6.5 x 10-6 C-1
OF THE RESTIVITY
TENSILE STRENGTH
20-100 C)
4.5 x 10-3 C-1
SHEET
50 kpsi - 115 kpsi
HARDNESS
ROD
60 kpsi - 110 kpsi
SHEET
220 - 240 DPH
WIRE
90 kpsi - 350 kpsi
ROD
200 - 220 DPH
YIELD STRENGTH
WIRE
250 - 300 DPH
(0.2% OFFSET)
SHEET
40 kpsi - 95 kpsi
ROD
55 kpsi - 90 kpsi
WIRE
75 kpsi - 300 kpsi





AVAILABLE SIZES

SHEET
.050
.062
.078
.109
.125
.140



PLATE
.250
.375
.500
.750
1.00



COIL / FOIL
.003
.004
.005
.010
.015
.020
.030
.040
.050
.062


ROD
.125
.250
.312
.437
.500
.625
.750
.875
1.00
1.25
1.50
1.75
2.00
2.25
2.50
3.00
3.50
4.00

 

*NOTE: Other sizes available upon request.

 

[TOP]

 


Home | Site Map | Profile | Technical Data | Quote/Order | Contact Info | NEA Inside Newsletter
Literature | Metals Calculator | Directions | Price Vs. Quality | Compliance Certificates

Copyright © 2003 National Electronic Alloys, Inc